When sorting out the ponies I found that Tulip was a bit sticky to the touch - not majorly tacky but that sort of 'is she, isn't she' stickiness. I guess this might be the start of the plasticiser breaking down so I've removed her from the cabinet and put her in 'quarantine' on an open shelf in another room.
I've read the posts about VOCs on here - thanks for the information - 2 questions though
how large should a quarantine zone away from other ponies be? she's on an open shelf about 20cms from any other pony (my 2 old reprobates Poser Beachball and Peg-leg Moonstone live at the other end of the shelf, though they are handled a lot as they get to be models for craft stuff so I think I'd feel any stickiness quickly on them.) The room is airy and used a lot so well ventilated.
I know it's a difficult thing to answer as it all depends upon a combination of factors but about how long does it take for the plasticiser to leach - is quarantine likely to be weeks or months or years approximately?
the other thing is that the shelf catches afternoon sun through the window (UK sun only). Is Tulip a known tanner?
Thank you